High quality Kafuter K-5211 thermal grease CPU not curing thermal grease 1.2 thermal conductivity white 60g

  • Liquid silicone: The thermal grease is made of liquid silicone, which is more durable and flexible than other materials. you can use it with confidence.
  • Seller recommended: If you have any questions, please contact us at any time, we will provide the best service for you.
  • Clever design: The thermal conductive silicone sealant has a unique design, which is easy to install and disassemble. it can be used as a replacement for the old or damaged one.

Code: K-5211

Kafuter 60g K-5211 thermal grease CPU not curing thermal grease 1.2 thermal conductivity white

Features

This product uses imported raw materials and formulations production, use, thermal conductivity and good insulating metal oxide and an organic compound from the silicone grease-like paste. Product has excellent thermal conductivity, good electrical insulation, wide temperature (operating temperature -50 ~ + 200 ), good use of stability, low consistency and good workability. This non-toxic, non-corrosive, odorless, quit, do not dissolve.

use

Widely used in heat, filling or coating electronics, electrical appliances, components, to derive the heat generated by components. Such as the CPU and heat sink caulking, power transistor, between the thyristor, diode and the substrate (aluminum, copper) filling the contact of every nip, depending on the machine power amplifier tube and fins, refrigeration and other semiconductors. Lowering the operating temperature of the heat generating element.

Technical performance

Exterior White cream

Penetration (1 / 10mm, 25 ) 260 to 300

Specific gravity (g / cm3) 1.9 to 2.1

Oil from the degree (% .200 , 8h) ≤2.0

Volatile (% .200 , 8h) ≤2.0

Strength Breakdown Voltage (kv / mm) ≥10

Volume resistivity (Ω.cm) 4 × 1014

Thermal conductivity (w / m · k) ≥1.2

Usage: Clean the surface to be coated, remove oil, then heat conductivity silicon ester direct extrusion, uniform coating to the surface to be coated. Coating method may need to be applied by brush, knife or roller.

Note: The construction of the surface should be uniform coating when the coating is not better, but the premise of ensuring fill the gap surface coated with a thin layer can be.

Note: The above data are based on our extensive obtained experimental results are reliable. However, due to the diversity of application conditions of practical application are beyond our control, so users need to be tested before use in order to confirm whether the product is suitable.

Color

Weight